Nowadays, the shell of the worm gear reducer is generally selected from gray iron casting, or cast steel and steel plate welding, etc.

Nowadays, the shell of the worm gear reducer is generally selected from gray iron casting, or cast steel and steel plate welding, etc. In the selection of reducer shell materials should be selected according to the use of the reducer environment. Shell we generally have to do process treatment, but the welded shell requirements can not leakage, the surface requirements of smooth, flat, weld seam requirements neat.
Worm gear reducer in the worm material we generally choose is 45 # steel, after tempering 217-255, important occasions used is 42CrMo, after tempering 269-302, or 38CrMoAl, tempering treatment, and finally also ion nitriding treatment, and then fine grinding. The surface of the oil seal is quenched.
 